Flint Hills P5M6K-080 Polypropylene Random Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Flint Hills Resources
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills P5M6K-080 Polypropylene Random Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Clarified, Gamma Radiation Sterilizable. Product does not contain animal derived components. Phthalate-free.Applications: Injection molding: Disposable Syringes. This product is not recommended for autoclave sterilization processes in the presence of aqueous solutions.Information Provided by Flint Hills Resources
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 27 g/10 min
27 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 85
85
ASTM D785
Tensile Strength, Yield 31.0 MPa
4500 psi
ASTM D638
Elongation at Yield 14 %
14 %
ASTM D638
Flexural Modulus, 1% Secant 966 MPa
140000 psi
ASTM D790
Izod Impact, Notched 0.750 J/cm

@Temperature 23.0 °C
1.41 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Gardner Impact 27.0 J

@Temperature 23.0 °C
19.9 ft-lb

@Temperature 73.4 °F
ASTM D5420
Tangent Modulus 1000 MPa
145000 psi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 81.0 °C
178 °F
ASTM D648
Optical Properties Metric English Comments
Haze 13 %

@Thickness 1.27 mm
13 %

@Thickness 0.0500 in
ASTM D1003