Flint Hills P9H8M-058X Specialty Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer Flint Hills Resources
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills P9H8M-058X Specialty Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Does not contain animal derived components. Product is Phthalate-free. A low phosphorus content material.Applications: Extrusion coating. Suitable for silicone coating.Information provided by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.901 g/cc
0.0326 lb/in³
ASTM D1505
Melt Flow 53 g/10 min
53 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 87
87
ASTM D785
Tensile Strength, Yield 29.0 MPa
4210 psi
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 1.13 GPa
164 ksi
Tangent; ASTM D790
Flexural Modulus, 1% Secant 1070 MPa
155000 psi
ASTM D790
Izod Impact, Notched 0.200 J/cm
0.375 ft-lb/in
ASTM D256
Gardner Impact 2.00 J
1.48 ft-lb
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 86.0 °C
187 °F
ASTM D648
Descriptive Properties Value Comments
FDA 21 CFR 177.1520(c) 1.1a and 2.2