Flint Hills P9H9Z-018 Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer Flint Hills Resources
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills P9H9Z-018 Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Specialty polypropylene, UL certified, and FDA compliant.Applications: Extrusion coating.Former Huntsman polypropylene products are now produced by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.901 g/cc
0.0326 lb/in³
ASTM D1505
Melt Flow 110 g/10 min
110 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 37.0 MPa
5370 psi
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 1.39 GPa
202 ksi
1% Secant; ASTM D790
Izod Impact, Notched 0.200 J/cm
0.375 ft-lb/in
23° C; ASTM D256
Gardner Impact 1.00 J
0.738 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C
196 °F
ASTM D648