Flint Hills P9R6K-054 Random Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Flint Hills Resources
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills P9R6K-054 Random Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent clarity. High flow material. Product does not contain any animal derived components. Phthalate-free.Applications: Injection molding - High clarity applications. A replacement for PET, PS and PC high clarity applications.Information provided by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 35 g/10 min
35 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 97
97
ASTM D785
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Elongation at Yield 14 %
14 %
ASTM D638
Flexural Modulus 0.972 GPa
141 ksi
Tangent; ASTM D790
Flexural Modulus, 1% Secant 919 MPa
133000 psi
ASTM D790
Izod Impact, Notched 0.790 J/cm
1.48 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 78.0 °C
172 °F
ASTM D648
Optical Properties Metric English Comments
Haze 2.8 %

@Thickness 0.635 mm
2.8 %

@Thickness 0.0250 in
ASTM D1003
5.8 %

@Thickness 1.27 mm
5.8 %

@Thickness 0.0500 in
ASTM D1003
Descriptive Properties Value Comments
FDA 21 CFR 177.1520(c) 3.1a