Material Notes:
Random copolymer with antistat, clarified, and FDA compliant.Features: Excellent clarity, non-blushing, good impact resistance, and high stiffness.Applications: Injection molding: lab ware, food packaging, kitchenware, and good clarity.FDA Notes: 21 CFR 177.1520 (c)3.1Former Huntsman polypropylene products are now produced by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 10 g/10 min
10 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Yield 29.0 MPa
4210 psi
ASTM D638
Elongation at Break >= 500 %
>= 500 %
ASTM D638
Modulus of Elasticity 1.207 GPa
175.1 ksi
ASTM D638
Flexural Modulus 1.138 GPa
165.1 ksi
ASTM D790
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
23° C; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM D648
Optical Properties Metric English Comments
Haze <= 10 %
<= 10 %
0.025 in. Thickness; ASTM D1003(A)