Fluorseals PTFE 15% glass filled

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Manufacturer Fluorseals
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fluorseals PTFE 15% glass filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Improved compressive strength and wear resistance.Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials.
Physical Properties Metric English Comments
Density 2.21 g/cc
0.0798 lb/in³
ASTM 1457-62 T
Deformation 10 - 17 %
10 - 17 %
14 MPa, 100 h, 23°C; ASTM D621-59
Mechanical Properties Metric English Comments
Ball Indentation Hardness 29.0 MPa
4210 psi
ASTM 1457-62 T
Tensile Strength at Break 16.0 MPa
2320 psi
ASTM 1457-62 T
Elongation at Break 300 %
300 %
ASTM 1457-62 T
Coefficient of Friction, Dynamic 0.135 - 0.16
0.135 - 0.16
v = 1 m/s
0.14 - 0.18
0.14 - 0.18
v = 1.9 m/s
Abrasion 2.4
2.4
mm of depth after 200 hrs load duration; Partner Material ST 50
Thermal Properties Metric English Comments
CTE, linear 110 µm/m-°C

@Temperature 100 °C
61.1 µin/in-°F

@Temperature 212 °F
DIN 52328
Thermal Conductivity 0.350 W/m-K
2.43 BTU-in/hr-ft²-°F
DIN 52612
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
DIN 53482
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
DIN 53482