Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics 25% Liquid Caustic Soda Membrane Grade

Category Fluid
Manufacturer Formosa Plastics Corporation, USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics 25% Liquid Caustic Soda Membrane Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Formosa Plastics Corporation, USA
Component Elements Properties Metric English Comments
Iron, Fe <= 4.0 %
<= 4.0 %
ASTM E291
Na2O 18.6 - 20.23 %
18.6 - 20.23 %
ASTM E291
Descriptive Properties Value Comments
Composition <0.15%
NA2CO3, FTTC2418
<100 ppm
NaClO3, ASTM E1787
<200 ppm
NaCl, ASTM E1787
<80 ppm
Na2SO4, ASTM E1787
24-26%
NaOH, ASTM E291