Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics Formolene® 5144L Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® 5144L Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Homopolymer for Injection Molded Applications requiring Heat Resistance Formolene® 5144L is a highly isotactic, nucleated polypropylene homopolymer designed for consumer products and appliance applications that require high stiffness and long-term exposure to elevated temperatures. It has found success in home laundry and dishwasher applications. 5144L has earned a UL continuous service rating of 115 °C.Specimens were injection molded according to the conditions specified in ASTM D4101Information provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 5.0 g/10 min

@Temperature 230 °C
5.0 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength, Yield 40.0 MPa
5800 psi
2" (50mm) per min; ASTM D638
Elongation at Yield 5.5 %
5.5 %
2" (50mm) per min; ASTM D638
Flexural Modulus 2.00 GPa
290 ksi
1.3mm per min, 1% secant; ASTM D790
Izod Impact, Notched 0.267 J/cm

@Temperature 23.0 °C
0.500 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
257 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °C
151 °F
ASTM D648
Users viewing this material also viewed the following: