Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics Formolene® HP4401 Pipe HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® HP4401 Pipe HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Density Hexene CopolymerApplications: Potable water, industrial mining, oil and gas gatheringsFormolene HP4401 is a high performance copolymer that is designed for the most demanding requirements of pressure pipe applications. It has good long-term hoop strength performance, very high melt strength, outstanding toughness even at low temperatures.Produced using licensor formulation for HHM TR-480Z. Licensor does not warrant or imply that this product meets their specifications for HHM TR-480Z.Formolene HP4401 meets all the requirements of ASTM D4976-PE225. It also meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520 for food packaging.Nominal properties reported herein were determined on compression molded specimens prepared in accordance with Procedure C of ASTM D1928. Physical properties are typical of product but do not reflect normal testing variance and therefore should not be used for specification purposes.Information provided by Formosa Plastics Corporation, USA.
Physical Properties Metric English Comments
Density 0.944 g/cc
0.0341 lb/in³
Natural; ASTM D1505
0.955 g/cc
0.0345 lb/in³
Black; ASTM D1505
Environmental Stress Crack Resistance >= 1000 hour
>= 1000 hour
Condition A,B,C (100% Igepal), F<sub>50</sub>; ASTM D1693
Melt Flow 0.11 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.11 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
High Load Melt Index 12 g/10 min

@Load 21.6 kg,
Temperature 190 °C
12 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Condition F; ASTM D1238
Mechanical Properties Metric English Comments
PENT 150 hour
150 hour
ASTM F1473
Tensile Strength at Break 34.5 MPa
5000 psi
2" (50mm) per min.; ASTM D638 Type IV
Tensile Strength, Yield 22.1 MPa
3200 psi
2" (50mm) per min.; ASTM D638 Type IV
Elongation at Break >= 500 %
>= 500 %
2" (50mm) per min.; ASTM D638
Flexural Modulus 0.758 GPa
110 ksi
ASTM D3350
0.965 GPa
140 ksi
ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -90.0 °C
<= -130 °F
ASTM D746
Users viewing this material also viewed the following: