Material Notes:
CopolymerApplications: Thin wall containersInformation provided by Formosa Plastics Corporation, USA.
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ASTM D1505
Melt Flow 40 g/10 min
40 g/10 min
ASTM D1238