Formosa Plastics Formolene® LH5326 Injection Molding HDPE  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® LH5326 Injection Molding HDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CopolymerApplications: Housewares, bowls, food containers, toysFormolene LH5326 is a high density polyethylene for injection molding applications.Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.Information provided by Formosa Plastics Corporation, USA.
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
ASTM D1505
Melt Flow 26 g/10 min
26 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.1 MPa
3930 psi
ASTM D882
Flexural Modulus 0.903 GPa
131 ksi
ASTM D790