Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics Formolon® 113 PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolon® 113 PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PVC Copolymer Suspension Resin F-113 has been developed primarily to meet the processing requirements of the vinyl composition tile (VCT) manufacturers. In addition to vinyl floor tile industry, F-113 has found success in protective and strippable coatings.Information provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Bulk Density 0.560 g/cc
0.0202 lb/in³
ASTM D1895
Volatiles 0.30 %
0.30 %
ASTM D3030
Particle Mesh Size 40 Mesh
40 Mesh
99.9% thru; ASTM D1921B
Viscosity 0.48 cP
0.48 cP
Inherent; ASTM D1243
Relative Viscosity 1.55 cP
1.55 cP
QC-10-104
Vinyl Acetate Content 13 %
13 %
QC-10-105
Descriptive Properties Value Comments
K-Value 48
Fikentscher's Constant