Fujipoly Industries Zebra® Silver Connector

Category Polymer , Thermoset , Silicone
Manufacturer Fujipoly Industries
Trade Name Zebra®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fujipoly Industries Zebra® Silver Connector.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fujipoly New High performance Silver Zebra connectors are constructed of alternating parallel layers of electrically conductive and nonconductive silicone elastomer. The electrically conductive layer if filled with silver metal particles.Information provided by Fujipoly Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
Support Rubber
58
58
Insulating Layer
80
80
Conductive Layer
Tensile Strength, Yield 2.00 MPa
290 psi
Conductive Layer
4.00 MPa
580 psi
Support Rubber
7.70 MPa
1120 psi
Insulating Layer
Elongation at Yield 120 %
120 %
Conductive Layer
380 %
380 %
Insulating Layer
400 %
400 %
Support Rubber
Tear Strength 13.0 kN/m
74.2 pli
Conductive Layer
17.0 kN/m
97.0 pli
Insulating Layer
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 85.0 °C
185 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 0.00010 ohm-cm
0.00010 ohm-cm
Conductive Layer
1.00e+14 ohm-cm
1.00e+14 ohm-cm
Support Rubber
1.00e+14 ohm-cm
1.00e+14 ohm-cm
Insulating Layer
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
Between Layers
Descriptive Properties Value Comments
Color Light Blue
Support Rubber
Off-White
Insulating Layer
Silver Gray
Conductive Layer
Continuity Resistance <0.5 ohms
Current Carrying Capacity 700 mA
1.0mm pitch; 0.50mm by 0.50mm pad