GEHR Plastics PP Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer GEHR Plastics Inc
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF GEHR Plastics PP Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polypropylene shows a high mechanical strength and a tensile strength, but a low notched impact strength. PP resists stress cracking and it is easy to weld. At minus temperatures it can get brittle. The chemical and electrical properties are very good. The continuous operating temperatures ranges between 5°C and 100°C.Propertieslow weighthigh heat resistancehigh tensile strengthhigh surface strengthhigh chemical resistancelow oxidation resistancelow abrasion resistancebrittle in the coldnessHF-welding not possiblenatural color is not weather resistantApplicationspumpsvalvesgasketssupporting standsspacer for the platingparticles for toys
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ISO 1183
Water Absorption 0.010 %
0.010 %
ISO 62
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
DIN 53505
Ball Indentation Hardness 67.0 MPa
9720 psi
ISO 2039
Tensile Strength, Yield 30.0 MPa
4350 psi
ISO 527
Elongation at Break >= 50 %
>= 50 %
ISO 527
Elongation at Yield 10 %
10 %
ISO 527
Modulus of Elasticity 1.20 GPa
174 ksi
ISO 527
Charpy Impact Unnotched NB
NB
ISO 179
Charpy Impact, Notched 5.00 J/cm²
23.8 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C
205 °F
ISO 75
Vicat Softening Point 91.0 °C
196 °F
VST/B/50; ISO 306
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+16 ohm-cm
>= 1.00e+16 ohm-cm
VDE 0303
Dielectric Constant 2.3

@Frequency 1.00e+6 Hz
2.3

@Frequency 1.00e+6 Hz
DIN 53483
Dielectric Loss Index 0.00020

@Frequency 1.00e+6 Hz
0.00020

@Frequency 1.00e+6 Hz
DIN 53483
Descriptive Properties Value Comments
Acid Resistance yes
Aromatic Resistance no
Bondability yes
CKW Resistance limited
Color Grey
Hydrocarbonate Resistance yes
Hydroxide Resistance yes
Ketone Resistance yes
Physiological indifference according yes
Resistance Against Hot Water yes
UV Stabilization limited