Material Notes:
ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transparency. These products can be injection molded, and extruded.Information provided by Greater Eastern Resins Industrial Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
ASTM D2240
Tensile Strength 40.0 MPa
5800 psi
ASTM D412
Tensile Strength, Yield 15.0 MPa

@Strain 50.0 %
2180 psi

@Strain 50.0 %
ASTM D412
19.0 MPa

@Strain 100 %
2760 psi

@Strain 100 %
ASTM D412
33.0 MPa

@Strain 300 %
4790 psi

@Strain 300 %
ASTM D412
Elongation at Break 480 %
480 %
ASTM D412
Tear Strength 200 kN/m
1140 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 60
60
ASTM D1044(Taber) H-22