GRECO ISOTHANE 5085A Polyether TPU Resin

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer GRECO
Trade Name ISOTHANE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF GRECO ISOTHANE 5085A Polyether TPU Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ISOTHANE 5000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent bio-compatibility, hydrolytic resistance, fungus resistance, and low temperature performance properties. These products can be injection molded, blow molded, and extruded. These are used for biomedical and drug administration applications.Information provided by Greater Eastern Resins Industrial Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
ASTM D2240
Tensile Strength 39.0 MPa
5660 psi
ASTM D412
Tensile Strength, Yield 3.90 MPa

@Strain 50.0 %
566 psi

@Strain 50.0 %
ASTM D412
5.90 MPa

@Strain 100 %
856 psi

@Strain 100 %
ASTM D412
12.0 MPa

@Strain 300 %
1740 psi

@Strain 300 %
ASTM D412
Elongation at Break 540 %
540 %
ASTM D412
Tear Strength 500 kN/m
2850 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 20
20
ASTM D1044(Taber) H-22
Compression Set 30 %

@Temperature 23.0 °C,
Time 79200 sec
30 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
35 %

@Temperature 70.0 °C,
Time 79200 sec
35 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395