Garlock 19 SBR Rubber Gasketing, Cotton Reinforced

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Garlock Rubber Technologies
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock 19 SBR Rubber Gasketing, Cotton Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SBR rubber with cotton sheeting as fabric insertCombines elasticity and extensibility of rubber with strength of fabric insert. Specially compounded in varying burst strengths for almost any service conditionInformation provided by Garlock Rubber Technologies
Mechanical Properties Metric English Comments
Hardness, Shore A 75 - 85
75 - 85
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.3 °C

@Pressure 1.72 MPa
200 °F

@Pressure 250 psi
Electrical Properties Metric English Comments
Dielectric Strength 1.22 kV/mm

@Thickness 3.17 mm
31.0 kV/in

@Thickness 0.125 in
Unconditioned; ASTM D149
Descriptive Properties Value Comments
Color Black