Garlock 4160 Natural Sheet Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Garlock Rubber Technologies
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock 4160 Natural Sheet Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent general purpose gasket materials for air, hot and cold water, saturated steam and exterior service.Red, smooth finishInformation provided by Garlock Rubber Technologies
Mechanical Properties Metric English Comments
Hardness, Shore A 55 - 65
55 - 65
Tensile Strength >= 8.27 MPa
>= 1200 psi
9.65 MPa
1400 psi
Typical
Elongation at Break >= 400 %
>= 400 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.2 °C
180 °F
Minimum Service Temperature, Air -28.9 °C
-20.0 °F