Garlock 567 EPDM Sheet Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Garlock Rubber Technologies
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock 567 EPDM Sheet Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent general purpose gasket materials for air, hot and cold water, saturated steam and exterior service.Black, smooth finish, commercial qualityInformation provided by Garlock Rubber Technologies
Mechanical Properties Metric English Comments
Hardness, Shore A 55 - 65
55 - 65
Tensile Strength >= 6.89 MPa
>= 1000 psi
8.27 MPa
1200 psi
Typical
Elongation at Break >= 350 %
>= 350 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -28.9 °C
-20.0 °F