Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Garlock 681 Vegetable Fiber Gasketing

Category Polymer , Thermoplastic , Cellulosic
Manufacturer Garlock Rubber Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock 681 Vegetable Fiber Gasketing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vegetable fiber with glue-glycerin binder (branded).Style 681 is designed for use in lightweight flanges and is compatible with water and most hydrocarbons.Information provided by Garlock Rubber Technologies
Mechanical Properties Metric English Comments
Tensile Strength 13.8 MPa
2000 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C

@Pressure 1.38 MPa
212 °F

@Pressure 200 psi
Electrical Properties Metric English Comments
Dielectric Strength 0.827 kV/mm
21.0 kV/in
Unconditioned; ASTM D149
Users viewing this material also viewed the following: