Garlock 9064 Neoprene Sheet Rubber Gasketing

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Garlock Rubber Technologies
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock 9064 Neoprene Sheet Rubber Gasketing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Neoprene (CR)FDA-approved. Exceptional material for food plants, with superior resistance to most all food products; oily and aqueous.Information provided by Garlock Rubber Technologies
Mechanical Properties Metric English Comments
Hardness, Shore A 55 - 65
55 - 65
ASTM D 2240
Tensile Strength 16.5 MPa
2400 psi
ASTM F152
Elongation at Break >= 790 %
>= 790 %
ASTM D 395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C

@Pressure 1.72 MPa
250 °F

@Pressure 250 psi
Minimum Service Temperature, Air -28.9 °C
-20.0 °F
Compliance Properties Metric English Comments
FDA Yes
Yes
Descriptive Properties Value Comments
Color Off-White