Garlock 9405 PTFE Rubber Sheet, 25% Glass Filled

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Manufacturer Garlock Rubber Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock 9405 PTFE Rubber Sheet, 25% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Premium Grade 25% Glass-filled Skived PTFE SheetInformation provided by Garlock Rubber Technologies
Physical Properties Metric English Comments
Specific Gravity 2.15 - 2.22 g/cc
2.15 - 2.22 g/cc
Deformation 3.0 - 9.0 %

@Time 86400 sec,
Pressure 13.8 MPa
3.0 - 9.0 %

@Time 24.0 hour,
Pressure 2000 psi
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 56 - 68
56 - 68
ASTM D2240
Tensile Strength 6.89 - 20.7 MPa
1000 - 3000 psi
ASTM D638, ASTM D1709
Elongation at Break 50 - 250 %
50 - 250 %
ASTM D638, ASTM D1709
Compressive Strength 8.27 - 11.0 MPa
1200 - 1600 psi
0.2% Offset; ASTM D695
6.21 - 8.62 MPa

@Strain 1.00 %
900 - 1250 psi

@Strain 1.00 %
ASTM D695
Thermal Properties Metric English Comments
CTE, linear 54.0 - 144 µm/m-°C

@Temperature 25.6 - 204 °C
30.0 - 80.0 µin/in-°F

@Temperature 78.0 - 400 °F
ASTM D696
Thermal Conductivity 0.360 - 0.504 W/m-K
2.50 - 3.50 BTU-in/hr-ft²-°F
ASTM C177