Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Garlock 9800 Compressed Carbon Fiber Gasketing, SBR Binder

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Garlock Rubber Technologies
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock 9800 Compressed Carbon Fiber Gasketing, SBR Binder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Carbon fibers with a SBR binder.Carbon fiber gasketing excels in harshest conditions- intense heat, high pressure, saturated steam and hot oilsLaboratory tested for fire safetyMaintains effective seal during pressure and temperature fluctuationsSuperior torque retention lowers leakage rates and reduces maintenance timeMedia: Saturated steam, Water, Inert gases, Mild acids, Mild alkaliesInformation provided by Garlock Rubber Technologies
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0608 lb/in³
Permeability 0.015
0.015
Gas Permeability, cc/min; DIN 3535 Part 4
Mechanical Properties Metric English Comments
Tensile Strength 10.3 MPa
1500 psi
across grain; ASTM F152
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 482 °C
900 °F
Continuous
343 °C

@Pressure 13.8 MPa
650 °F

@Pressure 2000 psi
Continuous
Minimum Service Temperature, Air -73.3 °C
-100 °F
Descriptive Properties Value Comments
Compressibility, % 7-17
ASTM F36
Creep Relaxation, % 15
ASTM F38