Garlock GYLON® 3540 Microcellular PTFE Gasketing

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Garlock Rubber Technologies
Trade Name GYLON®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock GYLON® 3540 Microcellular PTFE Gasketing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Microcellular PTFE.Highly compressible PTFE seals under low bolt load- suitable for many non-metallic flangesCompressible material conforms to surface irregularities, especially on warped, pitted or scratched flangesReduced cold flow and creep normally associated with conventional PTFE gasketsMedia: Strong caustics, strong acids, hydrocarbons, chlorine, cryogenics, glass-lined equipmentInformation provided by Garlock Rubber Technologies
Physical Properties Metric English Comments
Density 2.05 g/cc
0.0741 lb/in³
estimated by MatWeb
Permeability 0.015
0.015
Gas Permeability, cc/min; DIN 3535 Part 4
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C

@Pressure 8.27 MPa
500 °F

@Pressure 1200 psi
Continuous
Minimum Service Temperature, Air -268 °C
-450 °F
Electrical Properties Metric English Comments
Dielectric Strength 2.40 kV/mm

@Temperature 121 °C,
Time 10800 sec
61.0 kV/in

@Temperature 250 °F,
Time 3.00 hour
0.125 in. thickness; ASTM D149
3.39 kV/mm

@Temperature 121 °C,
Time 10800 sec
86.0 kV/in

@Temperature 250 °F,
Time 3.00 hour
0.0625 in. thickness; ASTM D149
0.630 kV/mm

@Thickness 1.59 mm
16.0 kV/in

@Thickness 0.0625 in
100% RH for 96 hours; ASTM D149
Descriptive Properties Value Comments
Color White
Compressibility, % 70-85
ASTM F36
Creep Relaxation, % 10
ASTM F38
Sealability ASTM F37B, ml/hr 0.25
ASTM Fuel A