Garlock Klozure® Mill-Right® V FKM Oil Seal

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer
Manufacturer Garlock Rubber Technologies
Trade Name Klozure®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock Klozure® Mill-Right® V FKM Oil Seal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A proprietary formulation of Fluoroelastomer (FKM). Engineered specifically for high-performance applications that demand the tightest sealing system, longest service life, and constant operation within harsh chemical environments.Information provided by Garlock Rubber Technologies
Mechanical Properties Metric English Comments
Hardness, Shore A 76
76
Coefficient of Friction 1.158
1.158
Taber Abrasion, mg/1000 Cycles 40
40
ASTM D4060
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Continuous
232 °C
450 °F
Spike
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Processing Properties Metric English Comments
Shelf Life 120 Month
120 Month
Descriptive Properties Value Comments
Color Green