Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Garlock MULTI-SWELLâ„¢ 3760 Compressed Aramid Fiber Gasketing

Category Polymer , Thermoset , Aramid , Rubber or Thermoset Elastomer (TSE)
Manufacturer Garlock Rubber Technologies
Trade Name MULTI-SWELL™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock MULTI-SWELLâ„¢ 3760 Compressed Aramid Fiber Gasketing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Aramid fibers with a proprietary rubber binder.Creates compressive load in light weight flanges in oil and water serviceTwice as compressible as standard fiber gasketsSeals with low load and irregular surfacesEasy to cut and handle, extremely flexibleNuclear Regulatory Commission 10CFR 50 Appendix B CertifiedInformation provided by Garlock Rubber Technologies
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0492 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength 6.89 MPa
1000 psi
across grain; ASTM F152
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C

@Pressure 3.45 MPa
400 °F

@Pressure 500 psi
Continuous
Minimum Service Temperature, Air -73.3 °C
-100 °F
Electrical Properties Metric English Comments
Dielectric Strength >= 15.2 kV/mm

@Temperature 121 °C,
Time 10800 sec
>= 385 kV/in

@Temperature 250 °F,
Time 3.00 hour
0.0625 in. thickness; ASTM D149
<= 0.394 kV/mm

@Thickness 1.59 mm
<= 10.0 kV/in

@Thickness 0.0625 in
100% RH for 96 hours; ASTM D149
<= 0.394 kV/mm

@Thickness 3.17 mm
<= 10.0 kV/in

@Thickness 0.125 in
100% RH for 96 hours; ASTM D149
Descriptive Properties Value Comments
Color Blue/Off-White
Compressibility, % 15-30
ASTM F36
Creep Relaxation, % 30
ASTM F38
Sealability ASTM F37B, ml/hr 0.15
ASTM Fuel A
0.2
Nitrogen
Users viewing this material also viewed the following: