Garlock Super Rinohideâ„¢ 7160 SBR Rubber Lining

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Garlock Rubber Technologies
Trade Name Super Rinohide™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock Super Rinohideâ„¢ 7160 SBR Rubber Lining.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SBR rubber lining for protection applications such as chute lining and skirtboards.Super RINOHIDEâ„¢, in particular, performs with superior resistance to abrasion, impact, aging and weathering. It is made of specially compounded SBR to withstand severe impact and abrasion.Information provided by Garlock Rubber Technologies
Mechanical Properties Metric English Comments
Hardness, Shore A 55 - 65
55 - 65
Tensile Strength >= 17.2 MPa
>= 2500 psi
19.3 MPa
2800 psi
Typical
Elongation at Break >= 500 %
>= 500 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.3 °C
200 °F
Minimum Service Temperature, Air -28.9 °C
-20.0 °F