Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gharda Chemicals GATONE™ 5300PF Polyetheretherketone (PEEK)  (discontinued **)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Unreinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gharda Chemicals GATONE™ 5300PF Polyetheretherketone (PEEK)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric Strength, Volume Resistivity, Tracking Resistance Excellent Radiation Resistance Applications:Medical appliances including implantationAerospace applicationEngineering applications like compressor plates, valve seats, moving parts for textile machines Electrical and communication cables Scientific laboratory instruments Information provided by Gharda ChemicalsSolvay Advanced Polymers completed its acquisition of this product line in May 2006.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Volatiles 0.50 %
0.50 %
by TGA
Viscosity Test 0.90 cm³/g
0.90 cm³/g
Inherent, 0.5% solution in 98%H2SO4; ASTM D2857
Mechanical Properties Metric English Comments
Tensile Strength, Yield 90.0 MPa
13100 psi
ASTM D638
Elongation at Break >= 50 %
>= 50 %
ASTM D638
Tensile Modulus 3.50 GPa
508 ksi
ASTM D638
Flexural Strength 145 MPa
21000 psi
ASTM D790
Flexural Modulus 3.50 GPa
508 ksi
ASTM D790
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 340 °C
644 °F
DSC
Glass Transition Temp, Tg 145 °C
293 °F
DSC
Processing Properties Metric English Comments
Moisture Content 0.20 %
0.20 %
P/QA/I/043