Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gharda Chemicals GATONE™ 5630GF Polyetheretherketone (PEEK)  (discontinued **)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Glass Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gharda Chemicals GATONE™ 5630GF Polyetheretherketone (PEEK)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric Strength, Volume Resistivity, Tracking Resistance Excellent Radiation Resistance Applications:Medical appliances including implantationAerospace applicationEngineering applications like compressor plates, valve seats, moving parts for textile machines Electrical and communication cables Scientific laboratory instruments Information provided by Gharda ChemicalsSolvay Advanced Polymers completed its acquisition of this product line in May 2006.
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Filler Content 30 %
30 %
Water Absorption 0.080 %
0.080 %
24 Hours; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 102
102
ASTM D785
Tensile Strength, Yield 160 MPa
23200 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Tensile Modulus 10.0 GPa
1450 ksi
ASTM D638
Flexural Strength 260 MPa
37700 psi
ASTM D790
Flexural Modulus 10.0 GPa
1450 ksi
ASTM D790
Izod Impact, Notched 0.950 J/cm
1.78 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 13.0 µm/m-°C

@Temperature 20.0 °C
7.22 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Maximum Service Temperature, Air 260 °C
500 °F
Continuous Use; UL-746B
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
ASTM D648
Glass Transition Temp, Tg 148 °C
298 °F
ASTM D3482
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
UL 94
Oxygen Index 45 %
45 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+16 ohm-cm
>= 1.00e+16 ohm-cm
ASTM D257
Surface Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
ASTM D257
Dielectric Constant 2.9

@Frequency 60 Hz
2.9

@Frequency 60 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D149
Dissipation Factor 0.0030

@Frequency 60 Hz
0.0030

@Frequency 60 Hz
ASTM D150
Comparative Tracking Index 150 V
150 V
ASTM D3638