Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gharda Chemicals GATONE™ PEEK, 30% Carbon Fiber Reinforced  (discontinued **)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gharda Chemicals GATONE™ PEEK, 30% Carbon Fiber Reinforced  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
GATONE™ PEEK grades with carbon fiber reinforcements ranging from 10- 40 % are available in natural or desired color. Custom made grades can be developed to meet specific requirements.CHARACTERISTICS: Outstanding chemical resistance.Outstanding wear resistance.Outstanding resistance to hydrolysis.Excellent mechanical properties.Outstanding thermal properties.Very good dielectric strength, volume resistivity, tracking resistance.Very good radiation resistance.Information provided by Gharda.Solvay Advanced Polymers completed its acquisition of this product line in May 2006.
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
ISO 118
Filler Content 30 %
30 %
Moisture Absorption at Equilibrium 0.060 %
0.060 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 244 MPa
35400 psi
ISO 527
Tensile Modulus 13.0 GPa
1890 ksi
ISO 527
Flexural Strength 355 MPa
51500 psi
ISO 178
Flexural Modulus 20.0 GPa
2900 ksi
ISO 178
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
(Expected) Continuous use, UL
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
ISO 75
Glass Transition Temp, Tg 148 °C
298 °F
DSC
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in