Gharda Chemicals Gafone™ 3100 Polyethersulfone (PES)  (discontinued **)

Category Polymer , Thermoplastic , Polyethersulfone (PES)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gharda Chemicals Gafone™ 3100 Polyethersulfone (PES)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: Excellent Thermal Resistance - Tg 224°C Outstanding Mechanical, Electrical, Flame & Chemical Resistance Very good Hydrolytic & Sterilization Resistance Good Optical Clarity Processed by all Conventional Techniques Applications: Clear applications like baby bottle, snuffer buttons, tee lights etc. Membrane applications Industrial and domestic coating Medical - Sterilizable box, surgical instrument Automotive - engine components Household - microwave oven food trays Industrial - oil level indicator, high temp. lighting fixture, Heat exchanger parts Electrical - Printed circuit board Information provided by Gharda ChemicalsSolvay Advanced Polymers completed its acquisition of this product line in May 2006.
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Water Absorption 0.56 %
0.56 %
24 Hours; ASTM D570
Melt Flow 10 - 13 g/10 min

@Load 2.16 kg,
Temperature 380 °C
10 - 13 g/10 min

@Load 4.76 lb,
Temperature 716 °F
6`; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 91.0 MPa
13200 psi
ASTM D638
Elongation at Break >= 50 %
>= 50 %
ASTM D638
Tensile Modulus 2.60 GPa
377 ksi
ASTM D638
Flexural Strength 124 MPa
18000 psi
ASTM D790
Flexural Modulus 2.70 GPa
392 ksi
ASTM D790
Izod Impact, Notched 0.700 J/cm
1.31 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 57.0 µm/m-°C

@Temperature 20.0 °C
31.7 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Maximum Service Temperature, Air 180 °C
356 °F
Continuous Use; UL-746B
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ASTM D648
Glass Transition Temp, Tg 225 °C
437 °F
ASTM D3482
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
UL 94
Oxygen Index 40 %
40 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+16 ohm-cm
>= 1.00e+16 ohm-cm
ASTM D257
Surface Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
ASTM D257
Dielectric Constant 3.2

@Frequency 60 Hz
3.2

@Frequency 60 Hz
ASTM D150
Dielectric Strength 16.0 kV/mm
406 kV/in
ASTM D149
Dissipation Factor 0.0040

@Frequency 60 Hz
0.0040

@Frequency 60 Hz
ASTM D150
Arc Resistance 50 sec
50 sec
ASTM D495
Comparative Tracking Index 150 V
150 V
ASTM D3638