Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gharda Chemicals Gafone S 1500 Polysulfone (PS)  (discontinued **)

Category Polymer , Thermoplastic , Polysulfone (PSU)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gharda Chemicals Gafone S 1500 Polysulfone (PS)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: High Temperature Resistance - Tg 189°C Excellent Clarity Excellent Mechanical & Electrical properties Easy to process Very good Hydrolytic Resistance Applications: Electrical & Electronic - Head lamp reflectors, Chip tray carriers, battery cases Industrial - Milking machine parts, Safety belts Medical - Surgical tools, Dialysis membranes Membrane applications Information provided by Gharda ChemicalsSolvay Advanced Polymers completed its acquisition of this product line in May 2006.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Water Absorption 0.30 %
0.30 %
24 Hours; ASTM D570
Melt Flow 38.44 - 49.6 g/10 min

@Load 5.00 kg,
Temperature 345 °C
38.44 - 49.6 g/10 min

@Load 11.0 lb,
Temperature 653 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.0 MPa
10900 psi
ASTM D638
Elongation at Break 50 - 100 %
50 - 100 %
ASTM D638
Tensile Modulus 2.70 GPa
392 ksi
ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 40.3 µm/m-°C

@Temperature 20.0 °C
22.4 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Maximum Service Temperature, Air 160 °C
320 °F
Continuous Use; UL-746B
Deflection Temperature at 1.8 MPa (264 psi) 170 °C
338 °F
ASTM D648
Glass Transition Temp, Tg 187 °C
369 °F
ASTM D3482
Flammability, UL94 V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
UL 94
Oxygen Index 31 %
31 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+16 ohm-cm
>= 1.00e+16 ohm-cm
ASTM D257
Surface Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
ASTM D257
Dielectric Constant 2.8

@Frequency 60 Hz
2.8

@Frequency 60 Hz
ASTM D150
Dielectric Strength 19.0 kV/mm
483 kV/in
ASTM D149
Dissipation Factor 0.0030

@Frequency 60 Hz
0.0030

@Frequency 60 Hz
ASTM D150
Arc Resistance 40 sec
40 sec
ASTM D495
Comparative Tracking Index 150 V
150 V
ASTM D3638
Copyright © lookpolymers.com All Rights Reserved