Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Glastic 1125 Corrosion-Resistant Panels

Category Polymer , Thermoset , Composite SMC , Filled/Reinforced Thermoset , Polyester, TS
Manufacturer Glastic
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Glastic 1125 Corrosion-Resistant Panels.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glastic® Corrosion-Resistant Panels are ideal for applications where resistance to both flame, and the splash or spill of laboratory chemicals is important. Glastic® Grade 1125 is asbestos-free, fiberglass-reinforced polyester resin sheet that offers low smoke generation when exposed to flame. This material has very low water absorption characteristics, along with excellent splash and spill resistance to acids, weak bases and aliphatic hydrocarbons. Grade 1125 is UL classified, has high strength, and has a bright white finish(no painting necessary). Some applications include fume hood liners, chemical storage cabinets and wall surfaces.Information provided by Glastic Corporation
Physical Properties Metric English Comments
Specific Gravity 1.81 g/cc
1.81 g/cc
ASTM D-792
Water Absorption 0.40 %
0.40 %
% by wt.; ASTM D-570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D-638
Tensile Modulus 11.7 GPa
1700 ksi
ASTM D-638
Flexural Strength 145 MPa
21000 psi
ASTM D-790
88.9 MPa

@Temperature 130 °C
12900 psi

@Temperature 266 °F
ASTM D-790
Compressive Strength 224 MPa
32500 psi
ASTM D-695
Izod Impact, Notched 4.48 J/cm
8.40 ft-lb/in
ASTM D-256
Thermal Properties Metric English Comments
CTE, linear 20.0 µm/m-°C

@Temperature 20.0 °C
11.1 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Thermal Conductivity 0.270 W/m-K
1.87 BTU-in/hr-ft²-°F
ASTM C-177
Flame Spread Index 20
20
Canadian Calculation; ASTM E-84
25
25
United States Calculation; ASTM E-84
Oxygen Index 35 %
35 %
ASTM D-2863
Descriptive Properties Value Comments
Smoke Developed 115
ASTM E-84
Standard Color White
UL Recognition File Number R9599
NEMA LI-1