Glastic GLASTHERM S Insulation Sheet

Category Polymer , Thermoset , Composite SMC , Filled/Reinforced Thermoset , Polyester, TS
Manufacturer Glastic
Trade Name GLASTHERM
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Glastic GLASTHERM S Insulation Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glastherm Grade S is a general purpose insulation sheet with an economical combination of thermal and physical properties. Not recommended for processes where the continuous operating temperature exceeds 425°F. Grade S is asbestos-free and rugged to withstand rough handling during installation. Suited to rubber molding industry.Information provided by Glastic Corporation
Physical Properties Metric English Comments
Density 1.84 g/cc
0.0665 lb/in³
ASTM D-792
Water Absorption 0.40 %
0.40 %
% by wt.; ASTM D-570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 94
94
ASTM D-785
Flexural Strength 124 MPa
18000 psi
ASTM D-790
Compressive Strength 68.9 MPa

@Temperature 288 °C
10000 psi

@Temperature 550 °F
ASTM D-695
79.3 MPa

@Temperature 200 °C
11500 psi

@Temperature 392 °F
ASTM D-695
110 MPa

@Temperature 150 °C
16000 psi

@Temperature 302 °F
ASTM D-695
310 MPa

@Temperature 23.9 °C
45000 psi

@Temperature 75.0 °F
ASTM D-695
Compressive Modulus 12.4 GPa
1800 ksi
ASTM D-695
Izod Impact, Notched 4.27 J/cm
8.00 ft-lb/in
ASTM D-256
Thermal Properties Metric English Comments
CTE, linear 11.0 µm/m-°C

@Temperature 20.0 °C
6.11 µin/in-°F

@Temperature 68.0 °F
Across Surface; ASTM D-696
70.2 µm/m-°C

@Temperature 20.0 °C
39.0 µin/in-°F

@Temperature 68.0 °F
Across Thickness; ASTM D-696
Thermal Conductivity 0.260 W/m-K
1.80 BTU-in/hr-ft²-°F
ASTM C-177
Maximum Service Temperature, Air 218 °C
425 °F
Flammability, UL94 HB

@Thickness 23.9 mm
HB

@Thickness 0.940 in
Electrical Properties Metric English Comments
Dielectric Strength 2.00 kV/mm
50.8 kV/in
Perpendicular S/T in Air; ASTM D-149
Descriptive Properties Value Comments
Standard Color Tan
Thickness Tolerance in ± 0.002