Glastic Laminates/Shapes UTR Pultruded Tubing, Fiberglass-Reinforced Polyester

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer Glastic
Trade Name Laminates/Shapes
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Glastic Laminates/Shapes UTR Pultruded Tubing, Fiberglass-Reinforced Polyester.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Glastic Corporation.NEMA GPO-3, NEMA LI-1. Commonly used for tubing and fuse applications.
Physical Properties Metric English Comments
Water Absorption 0.60 %
0.60 %
ASTM D570
Thermal Properties Metric English Comments
UL RTI, Electrical 130 °C
266 °F
UL 746B
UL RTI, Mechanical with Impact 160 °C
320 °F
UL 746B
Oxygen Index 30 %
30 %
ASTM D2862
Electrical Properties Metric English Comments
Arc Resistance 150 sec
150 sec
ASTM D495