Glastic Laminates/Shapes UTS Fiberglass-Reinforced Polyester Laminate

Category Polymer , Thermoset , Composite SMC , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer Glastic
Trade Name Laminates/Shapes
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Glastic Laminates/Shapes UTS Fiberglass-Reinforced Polyester Laminate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Glastic Corporation.NEMA GPO-2.
Mechanical Properties Metric English Comments
Flexural Strength 170 MPa
24700 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 155 °C
311 °F
NEMA temperature
UL RTI, Electrical 130 °C
266 °F
UL RTI, Mechanical with Impact 160 °C
320 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Arc Resistance 130 sec
130 sec
ASTM D495