Glastic T-160 Fiberglass-Reinforced Polyester Laminate

Category Polymer , Thermoset , Composite SMC , Filled/Reinforced Thermoset , Polyester, TS
Manufacturer Glastic
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Glastic T-160 Fiberglass-Reinforced Polyester Laminate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Grade T-160 is a new, high-strength, heat-resistant laminate. This highly creep-resistant material is excellent for applications where electrically insulating materials are subject to physical loading and moderately high temperature. NEMA grade GPO-1.Information provided by Glastic Corporation
Physical Properties Metric English Comments
Specific Gravity 1.90 g/cc
1.90 g/cc
ASTM D-792
Water Absorption 0.30 %
0.30 %
% by wt.; ASTM D-570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 96.5 MPa
14000 psi
ASTM D-638
Flexural Strength 200 MPa
29000 psi
ASTM D-790
172 MPa

@Temperature 130 °C
25000 psi

@Temperature 266 °F
ASTM D-790
Compressive Strength 386 MPa
56000 psi
ASTM D-695
Adhesive Bond Strength 12.3 MPa
1790 psi
ASTM D-229
Izod Impact, Notched 6.41 J/cm
12.0 ft-lb/in
ASTM D-256
Thermal Properties Metric English Comments
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Strength 16.2 kV/mm
411 kV/in
Perpendicular in Oil; ASTM D-149
19.6 kV/mm
498 kV/in
Perpendicular in Air; ASTM D-149
Arc Resistance 140 sec
140 sec
ASTM D-495
Descriptive Properties Value Comments
Electric Strength kV, ASTM D149 15
Parallel 48/50
40
Parallel as rec`d
Standard Color Natural