Global B-5200 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Global Polymers Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global B-5200 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description-has excellent stiffness thus requires less material to make blow moldingApplications-food containers, drinking bottles, medicine bottles, water containersInformation provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Density 0.966 g/cc
0.0349 lb/in³
ASTM D1505
Environmental Stress Crack Resistance 40 hour
40 hour
ASTM D1693
Melt Flow 0.35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Ultimate 34.3 MPa
4980 psi
ASTM D638
Tensile Strength, Yield 31.4 MPa
4550 psi
ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
Flexural Modulus 1.08 GPa
156 ksi
Olsen Stiffness; ASTM D747
Izod Impact, Notched 4.90 J/cm
9.18 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 134 °C
273 °F
ASTM D2117
Vicat Softening Point 128 °C
262 °F
ASTM D1525