Global GPEI-210 10% Glass Filled Reinforced, Polyetherimide

Category Polymer , Thermoplastic , Polyetherimide (PEI) , Polyetherimide (PEI), 10% Glass Fiber
Manufacturer Global Polymers Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global GPEI-210 10% Glass Filled Reinforced, Polyetherimide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Melt Flow 6.3 g/10 min

@Load 6.60 kg,
Temperature 337 °C
6.3 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 114 MPa
16500 psi
ASTM D638
Flexural Modulus 4.48 GPa
650 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Users viewing this material also viewed the following: