Global GX-92 PPO Polyphenylene Ether + PS

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer Global Polymers Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global GX-92 PPO Polyphenylene Ether + PS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Global Polymers
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
23/23°C; ASTM D792
Linear Mold Shrinkage, Flow 0.0090 cm/cm
0.0090 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 59.6 MPa
8650 psi
ASTM D638
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Izod Impact, Notched 1.87 J/cm
3.50 ft-lb/in
ASTM D256
Descriptive Properties Value Comments
Forms Pellets