Global MB-6366 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Global Polymers Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global MB-6366 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description-high density for high quality, excellent creep & chemical resistanceApplications-drinking water pipe, industrial pipe, sewer pipeInformation provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Density 0.961 g/cc
0.0347 lb/in³
ASTM D1505
Environmental Stress Crack Resistance 2000 hour
2000 hour
ASTM D1693
Carbon Black Loading 2.0 %
2.0 %
ASTM D4218
Melt Flow 0.060 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.060 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
0.40 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.40 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
ASTM D2240
Tensile Strength, Ultimate 29.4 MPa
4270 psi
ASTM D638
Tensile Strength, Yield 22.6 MPa
3270 psi
ASTM D638
Elongation at Break 600 %
600 %
ASTM D638
Flexural Modulus 0.785 GPa
114 ksi
Olsen Stiffness; ASTM D747
Izod Impact, Notched 3.92 J/cm
7.35 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 128 °C
262 °F
ASTM D2117
Vicat Softening Point 122 °C
252 °F
ASTM D1525