Goodfellow Aluminum 99/Silicon 1 Alloy

Category Metal , Nonferrous Metal , Aluminum Alloy
Manufacturer Goodfellow
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Aluminum 99/Silicon 1 Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
An addition of 1% Silicon lowers the melting range without producing brittleness. Aluminum/Silicon alloys are used in brazing alloys and welding wire for joining Aluminum as well as bonding wire in the semi-conductor industry.Information provided by Goodfellow.
Physical Properties Metric English Comments
Density 2.70 g/cc
0.0975 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 310 MPa
45000 psi
Thermal Properties Metric English Comments
Melting Point 600 °C
1110 °F
Component Elements Properties Metric English Comments
Aluminum, Al 99 %
99 %
Silicon, Si 1.0 %
1.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000260 - 0.00000350 ohm-cm
0.00000260 - 0.00000350 ohm-cm
Temperature Coefficient of 0.0042/K