Material Notes:
Information provided by Goodfellow.
Physical Properties Metric English Comments
Density 2.62 g/cc
0.0947 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 550 MPa
79800 psi
Longitudinal
Tensile Strength, Yield 500 MPa
72500 psi
Elongation at Break 2.3 %
2.3 %
Tensile Modulus 100 GPa
14500 ksi
Component Elements Properties Metric English Comments
Aluminum, Al 81 %
81 %
Copper, Cu 1.2 %
1.2 %
Lithium, Li 2.0 %
2.0 %
Magnesium, Mg 0.80 %
0.80 %
SiC 15 %
15 %
Descriptive Properties Value Comments
Volume Fraction SiC, % 13