Goodfellow Cellophane, Rayophane Regenerated Cellulose Film

Category Polymer , Film , Renewable/Recycled Polymer , Thermoplastic , Cellulosic
Manufacturer Goodfellow
Trade Name Cellophane, Rayophane
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Cellophane, Rayophane Regenerated Cellulose Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All forms of cellulose degrade before they melt but natural cellulose can be regenerated by the xanthate process to manufacture fibres, commonly called rayon or viscose, and film, commonly called by its earliest brand name Cellophane®. The latter films are plasticized by glycols and water to overcome their brittleness and are transparent, colorless and of moderate crystallinity. They were very widely used for packaging but have been substantially replaced by synthetic thermoplastics, especially polypropylene.They have very high permeability to moisture and, especially when dry, very low permeabiltiy to permanent gases. Their moisture content varies greatly with their environment reaching approximately 50% at 100% relative humidity. Not surprisingly, this causes many of their properties to vary considerably - so summarized values must be treated with considerable caution.Information provided by Goodfellow.
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
Water Absorption 50 %
50 %
Oxygen Transmission 0.350 - 3.50 cc-mm/m²-24hr-atm
0.889 - 8.89 cc-mil/100 in²-24hr-atm
Nitrogen Transmission 1.75 - 5.25 cc-mm/m²-24hr-atm
4.44 - 13.3 cc-mil/100 in²-24hr-atm
Carbon Dioxide Transmission 0.350 - 4.40 cc-mm/m²-24hr-atm
0.889 - 11.2 cc-mil/100 in²-24hr-atm
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.0 MPa
7980 psi
Transverse
120 MPa
17400 psi
Longitudinal
Elongation at Break 18 %
18 %
Longitudinal
55 %
55 %
Transverse
Modulus of Elasticity 3.00 GPa
435 ksi
Transverse
Tensile Modulus 5.00 GPa
725 ksi
Longitudinal
Thermal Properties Metric English Comments
Specific Heat Capacity 1.40 J/g-°C
0.335 BTU/lb-°F
Thermal Conductivity 0.0600 W/m-K
0.416 BTU-in/hr-ft²-°F
Fiber
Oxygen Index 18 %
18 %
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+10 - 1.00e+12 ohm-cm
1.00e+10 - 1.00e+12 ohm-cm
Dielectric Constant 4.0
4.0
Dry
Dielectric Strength 30.0 - 50.0 kV/mm

@Thickness 1.00 mm
762 - 1270 kV/in

@Thickness 0.0394 in
Dissipation Factor 0.060

@Frequency 1000 Hz
0.060

@Frequency 1000 Hz
Descriptive Properties Value Comments
Chemical Resistance - Alkalis Good
Chemical Resistance - Dilute Acids Good
Chemical Resistance - Greases and Oils Good
Permeability to Carbon Dioxide @25°C 0.004-0.05 x 10-13 cm3.cm cm-2 s-1 Pa -1
Permeability to Hydrogen 0.88 - 4.4 cc-mm/m²-24hr-atm
Permeability to Hydrogen @25°C 0.01-0.05 x 10-13 cm3.cm cm-2 s-1 Pa -1
Permeability to Nitrogen @25°C 0.02-0.06 x 10-13 cm3.cm cm-2 s-1 Pa -1
Permeability to Oxygen @25°C 0.004-0.04 x 10-13 cm3.cm cm-2 s-1 Pa -1
Permeability to Water @25°C 20000 x 10-13 cm3.cm cm-2 s-1 Pa -1
Radiation Resistance Fair