Material Notes:
Information provided by Goodfellow.
Thermal Properties Metric English Comments
Melting Point 966 °C
1770 °F
Component Elements Properties Metric English Comments
Nickel, Ni 62 %
62 %
Silicon, Si 38 %
38 %