Goodfellow Niobium 56/Titanium 44 Alloy

Category Metal , Nonferrous Metal , Niobium Alloy , Refractory Metal
Manufacturer Goodfellow
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Niobium 56/Titanium 44 Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Goodfellow.
Thermal Properties Metric English Comments
Melting Point 2200 °C
3990 °F
Component Elements Properties Metric English Comments
Niobium, Nb (Columbium, Cb) 56 %
56 %
Titanium, Ti 44 %
44 %