Goodfellow Platinum 90/Rhodium 10 Thermocouple Alloy

Category Metal , Nonferrous Metal , Precious Metal , Platinum Alloy
Manufacturer Goodfellow
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Platinum 90/Rhodium 10 Thermocouple Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The positive element of the type S thermocouple. Type S thermocouples are characterized by a high degree of chemical inertness and stability at high temperatures. Often used as a standard for calibration of base metal thermocouples.Information provided by Goodfellow.
Physical Properties Metric English Comments
Density 19.97 g/cc
0.7215 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 90 - 165
90 - 165
Tensile Strength at Break 320 - 620 MPa
46400 - 89900 psi
Elongation at Break <= 35 %
<= 35 %
Thermal Properties Metric English Comments
Thermal Conductivity 38.0 W/m-K
264 BTU-in/hr-ft²-°F
Melting Point 1830 - 1855 °C
3330 - 3371 °F
Solidus 1830 °C
3330 °F
Liquidus 1855 °C
3371 °F
Component Elements Properties Metric English Comments
Platinum, Pt 90 %
90 %
Rhodium, Rh 10 %
10 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000184 - 0.0000192 ohm-cm
0.0000184 - 0.0000192 ohm-cm
Temperature Coefficient of 0.0017/K