Goodfellow TZM Molybdenum High Temperature Alloy

Category Metal , Nonferrous Metal , Molybdenum Alloy
Manufacturer Goodfellow
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow TZM Molybdenum High Temperature Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Increased high temperature strength over pure molybdenum although, like Molybdenum, it oxidizes rapidly in oxidizing atmospheres above 500°CInformation provided by Goodfellow.
Physical Properties Metric English Comments
Density 10.22 g/cc
0.3692 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 560 - 1150 MPa
81200 - 167000 psi
Elongation at Break <= 20 %
<= 20 %
Tensile Modulus 320 GPa
46400 ksi
Thermal Properties Metric English Comments
CTE, linear 5.30 µm/m-°C

@Temperature 20.0 - 1000 °C
2.94 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 126 W/m-K
874 BTU-in/hr-ft²-°F
Melting Point 2500 - 2600 °C
4530 - 4710 °F
Solidus 2500 °C
4530 °F
Liquidus 2600 °C
4710 °F
Maximum Service Temperature, Air 400 °C
752 °F
Component Elements Properties Metric English Comments
Molybdenum, Mo 99 %
99 %
Titanium, Ti 0.50 %
0.50 %
Zirconium, Zr 0.10 %
0.10 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000530 - 0.00000550 ohm-cm
0.00000530 - 0.00000550 ohm-cm