Material Notes:
Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because this material contains a high percentage of sillimanite, it has a very good thermal shock resistance together with a very good slag resistance. This material is especially applicable in burner throats under severe conditions.Remarks: The stated chemical composition and physical properties represent average values.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.15 - 2.25 g/cc
0.0777 - 0.0813 lb/in³
After drying at 110°C
Thermal Properties Metric English Comments
Thermal Conductivity 0.730 - 0.830 W/m-K

@Temperature 100 °C
5.07 - 5.76 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.880 - 0.980 W/m-K

@Temperature 600 °C
6.11 - 6.80 BTU-in/hr-ft²-°F

@Temperature 1110 °F
1.07 - 1.27 W/m-K

@Temperature 1400 °C
7.43 - 8.81 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Maximum Service Temperature, Air 1600 °C
2910 °F
Shrinkage -0.300 - 0.300 %

@Temperature 1400 °C
-0.300 - 0.300 %

@Temperature 2550 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 59 %
59 %
Fe2O3 1.5 %
1.5 %
SiO2 36 %
36 %
Descriptive Properties Value Comments
Bonding Type ceramic
Material Consumption per 1 m3 2150 kg
Mixing Water 10-12 liters
per 100 kgs dry material
Segercone 35