Material Notes:
Description: This high refractory ramming material contains several well defined corundum qualities and only a small quantity of binding agent. Curas 90 has a very good resistance against erosion and corrosion. It's specially applied in electric arc furnace roofs.Remarks: The stated chemical composition and physical properties represent average values.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.70 - 2.80 g/cc
0.0975 - 0.101 lb/in³
After drying at 110°C
Thermal Properties Metric English Comments
Thermal Conductivity 2.30 - 2.40 W/m-K

@Temperature 100 °C
16.0 - 16.7 BTU-in/hr-ft²-°F

@Temperature 212 °F
2.35 - 2.45 W/m-K

@Temperature 1600 °C
16.3 - 17.0 BTU-in/hr-ft²-°F

@Temperature 2910 °F
2.45 - 2.55 W/m-K

@Temperature 600 °C
17.0 - 17.7 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Maximum Service Temperature, Air 1760 °C
3200 °F
Shrinkage -1.20 - 0.800 %

@Temperature 1600 °C
-1.20 - 0.800 %

@Temperature 2910 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 91 %
91 %
Fe2O3 0.30 %
0.30 %
SiO2 7.0 %
7.0 %
Descriptive Properties Value Comments
Bonding Type ceramic
Material Consumption per 1 m3 2900 kg
Segercone 41
Workability 20-25%
ASTM C181-176